Thin Films Demonstration
This demonstration is a product of Nanodays and NISE Network (Nisenet.org). Included in your kit is a guide with directions and information on how nanotechnology is involved. |
|
|
In this demonstration you have a shallow container, black paper, clear nail polish, permanent marker, and a peacock feather. |
|||||||||||||||||||||||||||||||||||||||||||
|
|
Write your name on a strip of black paper. | |||||||||||||||||||||||||||||||||||||||||||
|
|
Fill the shallow container with water. Slide the paper into the container. | |||||||||||||||||||||||||||||||||||||||||||
|
|
Make sure the paper is completely under water. | |||||||||||||||||||||||||||||||||||||||||||
|
|
Drip one drop of nail polish onto the surface of the water. The polish will spread out into a thin film. |
|||||||||||||||||||||||||||||||||||||||||||
|
|
Hold one end of the paper and lift it up out of the water. The film of nail polish will stick to the paper. Does the nail polish still look clear?
|
|||||||||||||||||||||||||||||||||||||||||||
|
_______________________________________ Check the Calendar for available dates! Teachers and educators may borrow these items for 7-day intervals. To borrow materials, please fill out 6 questions on this lending library request form. If you do not hear from us within 1 business day, please email This email address is being protected from spambots. You need JavaScript enabled to view it. . _______________________________________ |
|||||||||||||||||||||||||||||||||||||||||||
|
This demonstration meets the following California Science Standards: Life Science
Physical Science
Investigation and Experimentation
|