RET 2011: Manuel Casillas
![]() |
Intern: Manuel CasillasMentor: Stuart BrinkleyFaculty: Steve DenBaars |
Curriculum Overview
Chemical reactions are used to create specific shapes on surfaces of crystalline materials. This wet etching process is what scientists use to make up functional components within electronics. This lab helps students to understand how scientists sculpt tiny electrical components in an iPod.
Curriculum Developed:
(Please CLICK HERE for the Copyright Agreement.)
Wet Etching Process used in Nanotechnology |