EVG Plasma Activation System

Equipment Description:
Plasma Surface Activation
Manufacturer:
EVG Group
General Information and Usage:
This a capacitively coupled Oxygen plasma activation system used exclusively for the surface activation of clean surfaces prior to wafer bonding. This technique allows bonding temperatures to be lowered and is used as a companion tool to the Karl-Suss SB6 wafer bond tool.
Detailed Specifications:
- Gases used: O2 and N2
- Sample size: pieces to 6” wafer
Contact Information:
For additional information regarding the EVG system or if you would like to inquire about using the UCSB Nanofabrication Facility, please contact This email address is being protected from spambots. You need JavaScript enabled to view it. using the telephone number or e-mail address below.
This email address is being protected from spambots. You need JavaScript enabled to view it.
Phone: (805) 893-3918 ext. 208
E-Mail:
This email address is being protected from spambots. You need JavaScript enabled to view it.
Facility
Slides