NNIN Logo
Click here to see more pictures.
Teacher
School
Mentor
Faculty
Project
Marilyn Garza Santa Barbara Junior High Wendy Ibsen Mark Rodwell Integration of Nanoscale Education into Classrooms Through Inquiry and Laboratories
John Gomm Garden Street Academy Kevin Jiang Soraa, Inc.

Ammonothermal Growth of Ultra-Low Defect Gallium Nitride for LED and Power Electronic Applications

Raeanne Napoleon Santa Barbara City College Will Elliott Martin Moskovits

Micro-Multi-Junction Solar Cells in Anodized Aluminum

Rano Sidhu Rio Mesa High School Samuel Beach Luke Theogarajan

Ion Selective Chemistries for Nanoporous Anodized Alumina Based Selective Ion Pumps for Retinal and Neural Stimulation

Technical and educational staff services are possible through the generosity of the National Science Foundation through support via the NNIN.