The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility.  The system can do automated resistivity mapping for pieces to 8 inch wafers.  The resistivity range is 2mOhm/Square to 5MOhm/square.  Contour plots, 3D plots, histograms, data exporting are supported from the Windows XP based control system.

 

Contact Information:

For additional information regarding the CDE Resmap 4 Point Resistivity Mapper or if you would like to inquire about using the UCSB Nanofabrication Facility, please contact This email address is being protected from spambots. You need JavaScript enabled to view it. using the telephone number or e-mail address below. 

 

This email address is being protected from spambots. You need JavaScript enabled to view it.

Phone: (805) 893-3918 ext. 217

E-Mail: This email address is being protected from spambots. You need JavaScript enabled to view it.