Nanoproducts Home

Library Home

 

X-Satic Fabrics

 

 

What is it used for?

Clothes and other fabric materials.

 

What's nano about it?

Silver nanoparticles are integrated into the fabric and enhance the properties of the cloth.

 

How does it work?

Silver has an antimicrobial property which means that it inhibits bacteria from growing and producing waste. This gives the clothes an ant-odor property. the fabric is all natural, anti-static, therapeutic, and it has excellent heat transfer qualities. It has been testes for over 250 washes with no degradation in antimicrobial performance.

 

 

_______________________________________

Check the Nano Products Calendar for available dates!

Teachers and educators may borrow these items for 7-day intervals.

To borrow materials, please fill out 6 questions on this lending library request form.

If you do not hear from us within 1 business day, please email This email address is being protected from spambots. You need JavaScript enabled to view it..

_______________________________________

 

 

 

Technical and educational staff services are possible through the generosity of the National Science Foundation through support via the NNIN.